    Cobalt-Based Deformed Superalloy 15-53μ M Gh5188 3D Printing Powder

    Short Description:

    • Type: Alloy Steel Powder
    • Standard: ASTM, JIS, GB
    • Technique: 3D Printing/Laser Cladding
    • Mobility: ≤16s/50g
    • Bulk Density: ≥4.60g/cm3
    • Oxygen Content:≤200ppm
    • Nitrogen Content: ≤200ppm
    • Yield Strength /MPa: 900±50
    • Compressive Strength /MPa: 1000±50
    • Elongation /%: 13±2
    • Transport Package: III
    • Specification: 15-53μ m
    • Trademark: Fitech
    • Application: Tool Steel Bar

  • Molecular Formula: GH5188
  • Minimum Order: Depends on your requirement
  • USD$0.00
    • Quality First

      Quality First

    • Competitive Price

      Competitive Price

    • First-class Production Line

      First-class Production Line

    • Factory Origin

      Factory Origin

    • Customized Services

      Customized Services

    Anhui Fitech Material Co.,Ltd  has successfully certified by ISO 14001:2015 environmental management system,ISO 9001:2015 quality management system and ISO 45001 occupational health and safety certification. As a professional manufacturer and supplier, we have our own professional technology team to meet any of your requirements in quality and technology. If you want to buy Cobalt base alloy powder, Nickel base alloy powder, Ferro base alloy powder, Titanium base alloy powder, other 3D printing powder, or look for price quotation, please contact judy@fitechem.com

    company

    Features

    GH5188 is a solid solution strengthened cobalt based superalloy. The addition of 14% tungsten solid solution strengthened makes the alloy have excellent high temperature thermal strength. The addition of high chromium content and trace lanthanum makes the alloy have good high temperature oxidation resistance, and has satisfactory forming, welding and other technological properties.

    Main products GH4099
    Mobility 15-53μm ≤16s/50g
    Bulk density ≥4.60g/cm3
    Oxygen content ≤200ppm
    Nitrogen content ≤200ppm
    Mechanical property Compressive strength /Mpa 1000±50

    Yield strength /Mpa 900±50

    Elongation /% 13±2

    The alloy has good resistance to organic acid corrosion, but limited corrosion resistance in sulfuric acid and medium, in addition to the possibility of point corrosion in halides, has good corrosion resistance in oxidizing and non-oxidizing salts, and also has good corrosion resistance in water, vapor and mixtures of steam, air and carbon dioxide.

    test_pro_01

    Applications

    Aerospace;

    Laser cladding;

    Suitable for the manufacture of aeroengine parts requiring high strength below 980 ° C and oxidation resistance below 1100 ° C. It can also be used in space engines and space shuttles. Can produce and supply a variety of deformation products, such as sheet, medium plate, strip, bar, forgings, wire and precision castings.

    A N H U I F I T E C H M A T E R I A L C O . , L T D

    National Innovation Industrial Base Huguang Road, Shushan District, Hefei, Anhui, China

    Exhibition Show

    GUANGZHOU EXHIBITION

    Factory & Payment

    !FACTORY.FITECH
    transport2

    FAQs

    Q: Are you trading company or manufacturer ?
    A: We are factory.

    Q: How long is your delivery time?
    A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to
    quantity.

    Q: Do you provide samples ? is it free or extra ?
    A: Yes, we could offer the sample for free charge but do not pay the cost of freight.

    Q: What is your terms of payment ?
    A: Payment<=1000USD, 100% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shippment.

    Certificate

    certificate1
    certificate3
    ISO 9001
    ISO 14001
    ISO 45001
    index_cer3
    certificate4
    certificate5
    certificate6
    certificate7
    certificate8
    certificate9
    certificate10

    More products

    Water-Based Powder Sperical Stainless Steel 304L Metal Powder

    Water-Based Powder Sperical Stainless Steel 304...

    High-Strength Alloy Steel 4340 Powder Factory Price GB40crnimoa, Uns G43400, AISI/ASTM4340

    High-Strength Alloy Steel 4340 Powder Factory P...

    15-53μ M Laser Cladding Temperature Alloy Sperical Gh4099 Powder

    15-53μ M Laser Cladding Temperature Alloy Speri...

    China Provides Laser Cladding Powder M2 Powder for Additive Manufacturing

    China Provides Laser Cladding Powder M2 Powder ...

    Cobalt-Based Alloy Cobalt Chromium Molybdenum Alloy for Medical Dental Model

    Cobalt-Based Alloy Cobalt Chromium Molybdenum A...

    High Temperature Resistance TC4 Titanium Alloy 3D Printing/ Laser Cladding

    High Temperature Resistance TC4 Titanium Alloy ...